Mtareial | 38CrMoAIA,SACM645,AISI4140,SKD61,GHII3 |
---|---|
Nitriding Hardness | HV950-1200 |
Nitriding Depth | 0.5~0.8mm |
Quenching Hardness | HRC55-62 |
Nitriding Brittle | Less Than Grade 2 |
Surface Roughness | Ra0.4 |
---|---|
Warranty | 1 Year |
Material | 38CrMoAlA/Customized |
Nitriding Hardness | HV950-1050 |
Bimetallic Layer Nitriding Depth | 0.8-1.2mm |
Alloy Hardness | HRC55-62 |
---|---|
Surface Roughness | Ra0.4μm |
Basic Material | 38CrMoAlA/Customized |
Nitriding Layer Depth | 0.5-0.8 Mm |
Chromeplate Thickness | 0.05~0.10mm |
Basic Material | 38 CrMoAl A |
---|---|
Nitriding Hardness | ≥950HV |
Material | 38CrMoAlA, SKD61, 42CrMo, 9Cr18MoV |
Warranty | 1 Year |
Bimetallic Layer Thickness | 2-4mm |
Chromeplate Thickness | 0.05~0.10mm |
---|---|
Screw Diameter | Customized |
Cooling System | Water Cooling Or Oil Cooling |
Warranty | 12 Months |
Surface Roughness | Ra 0.4 |
Bimetallic Layer Thickness | 2-4mm |
---|---|
Nitriding Hardness | ≥950HV |
Nitriding Method | Gas Nitriding Or Plasma Nitriding |
Warranty | 1 Year |
Material | 38CrMoAlA, SKD61, 42CrMo, 9Cr18MoV |
Material | 38CrMoAlA, SKD61, 42CrMo, 9Cr18MoV |
---|---|
Nitriding Method | Gas Nitriding Or Plasma Nitriding |
Nitriding Depth | 0.5-0.8mm |
Nitride Brittleness | ≤Level 1 |
Chrome Plating Thickness | 0.03mm-0.08mm |
Chrome Plating Thickness | 0.03mm-0.08mm |
---|---|
Warranty | 1 Year |
Material | 38CrMoAlA, SKD61, 42CrMo, 9Cr18MoV |
Nitriding Hardness | ≥950HV |
Nitride Brittleness | ≤Level 1 |
Warranty | 1 Year |
---|---|
Basic Material | 38 CrMoAl A |
Nitriding Depth | 0.5-0.8mm |
Bimetallic Layer Thickness | 2-4mm |
Chrome Plating Thickness | 0.03mm-0.08mm |
Basic Material | 38 CrMoAl A |
---|---|
Screw Structure | Building Block Type, Integral Type |
Chrome Plating Thickness | 0.03mm-0.08mm |
Bimetallic Layer Thickness | 2-4mm |
Nitriding Method | Gas Nitriding Or Plasma Nitriding |