| Bimetallic Layer Depth | 0.8-3 Mm |
|---|---|
| Barrel Hardness | HRC58-62 |
| Tempering Hardness | HB260-290 |
| Straightness Of Screw | 0.015mm |
| Processing Technology | Nitriding Treatment |
| Straightness Of Screw | 0.015mm |
|---|---|
| Nitriding Hardness | 900-1000 HV |
| Processing Technology | Nitriding Treatment |
| Surface Roughness | Ra0.4 |
| Barrel Hardness | HRC58-62 |
| Heating Method | Ceramic Heater, Cast Aluminum Heater |
|---|---|
| Nitriding Method | Gas Nitriding Or Plasma Nitriding |
| Nitriding Depth | 0.5-0.8mm |
| Chrome Plating Thickness | 0.03mm-0.08mm |
| Material | 38CrMoAlA, SKD61, 42CrMo, 9Cr18MoV |
| Screw Structure | Building Block Type, Integral Type |
|---|---|
| Chrome Plating Thickness | 0.03mm-0.08mm |
| Warranty | 1 Year |
| Nitriding Method | Gas Nitriding Or Plasma Nitriding |
| Nitriding Depth | 0.5-0.8mm |
| Surface Roughness | Ra 0.4um |
|---|---|
| Nitriding Hardness | ≥900HV |
| Material | High-quality Alloy Steel |
| Surface Treatment | Nitriding/Bimetallic |
| Screw Diameter | Φ15mm-Φ300mm |
| Material | 38CrMoAlA,SKD61,42CrMo,DC53,Stainless Steel |
|---|---|
| Surface Treatment | Nitrided Treatment,Nitrided Or Bimetallic,Polishing/chrome Plating/PVD Coating,Bimetallic,Nitriding Treatment |
| Screw Design | Double-screw,Extruder Twin Screw Barrel,single Screw Barrel For Granulation Extruder,mini Screw Barrel |
| Application Machine | Screw Barrel Extruder,PE PP PVC WPC Profile Pipe Conical Twin Screw Barrel Extruder,Pelleting Extruder Spare Parts,SJSZ80/156 |
| Screw Diameter | 20~45MM,75/150mm,15mm-360mm,50-500MM,20-250 Mm L/D 15-50 Extruder Single Screw Barrel |
| Condition | New |
|---|---|
| Screw Length | 300-6000mm |
| Nitride Depth | 0.5-0.8mm |
| Screw Material | 38CrMoAlA, SACM645, 42CrMo, SKD61, DC53, Etc. |
| Feature | Wear And Corrosion Resistance |