| Tempering Hardness | HB260-290 |
|---|---|
| Nitriding Hardness | HV950-1050 |
| Depth Of Nitriding Layer | 0.4-0.7mm |
| Nitride Brittleness | ≤Level 1 |
| Surface Roughness | Ra0.4 |
| Material | 38CrMoAIA,SKD61,AISI4140,SACM645,,42CrMo |
|---|---|
| Quenching Hardness | HRC58-65 |
| Nitrided Brittleness | Less Than Grade 2 |
| Screw Straightness | 0.015mm |
| Alloy Depth | 2.0-3.0mm |
| Conventional Material | 38CrMoAlA SKD61 Cr12MoV SACM645 Ni-based-alloy GHII3 C276 |
|---|---|
| Warranty | 1 Year |
| Nitrided Hardness | HV950-1200 |
| Nitrided Depth | 0.5~0.8mm |
| Quenching Hardness | HRC55 ° - 62 ° |