| Kekerasan Tempering | HB260-290 |
|---|---|
| Kekerasan Nitridasi | HV950-1050 |
| Kedalaman lapisan nitriding | 0,4-0,7 mm |
| Brittleness nitride | ≤Level 1 |
| Kekasaran permukaan | Ra0.4 |
| Bahan | 38crmoaia, SKD61, AISI4140, SacM645 ,, 42CrMo |
|---|---|
| Kekerasan pendinginan | HRC58-65 |
| Kerapuhan Nitridasi | kurang dari kelas 2 |
| Kelurusan sekrup | 0,015mm |
| Kedalaman paduan | 2.0-3.0mm |
| Bahan konvensional | 38CRMOALA SKD61 CR12MOV SACM645 NI-ALLOY-ALLOY GHII3 C276 |
|---|---|
| Jaminan | 1 tahun |
| Kekerasan Nitrida | HV950-1200 |
| Kedalaman nitrided | 0,5 ~ 0,8mm |
| Kekerasan pendinginan | HRC55 ° - 62 ° |